Heat resistant steel castings hmanga hman theih temperature sang ber .
|
Nihna max a ni ..lum leh vawt tehna chhung boruak |
|||||
|
Hming |
A zat |
degree |
|||
|
- Ferrtic a ni. |
Gx30Crsi7 a ni. |
1.4710 |
750 |
||
|
GX40Crsi13 a ni. |
1.4729 |
850 |
|||
|
GX40Crsi17 a ni. |
1.4740 |
900 |
|||
|
Ferrtic leh Austenitic . |
Grade hrang hrang . |
GX40Crsi24 a ni. |
1.4745 |
1050 |
|
|
GX40Crsi28 a ni. |
1.4776 |
1150 |
|||
|
GX130Crsi29 a ni. |
1.4777 |
1100 |
|||
|
GX160Crsi18 a ni. |
1.4743 |
900 |
|||
|
GX40CRNISI27-4 a ni. |
1.4823 |
1100 |
|||
|
Austenitic 1000 a zir chhuak. |
GX25CRNISI18-9 ah a awm. |
1.4825 |
900 |
||
|
GX40CRNISI22-10 ah a awm. |
1.4826 |
950 |
|||
|
GX25CRNISI20-14 ah a awm. |
1.4832 |
950 |
|||
|
GX40CRNISI25-12 ah a awm. |
1.4837 |
1050 |
|||
|
GX40CRNISI25-20 a ni. |
1.4848 |
1100 |
|||
|
GX40CRNISINB24-24 ah hian a awm a. |
1.4855 |
1050 |
|||
|
GX35Nicsi25-21 ah a awm. |
1.4805 |
1000 |
|||
|
GX40NICRISSI35-17 ah a awm. |
1.4806 |
1000 |
|||
|
GX40NiCRSINB35-18 ah a awm. |
1.4807 |
1000 |
|||
|
GX40NICRISSI38-19 ah a awm. |
1.4865 |
1020 |
|||
|
GX40NiCRSINB38-19 ah hian a awm a. |
1.4849 |
1020 |
|||
|
GX10NiCRSINB32-20 ah hian a awm a. |
1.4859 |
1050 |
|||
|
GX40NICRISSI35-26 ah a awm. |
1.4857 |
1100 |
|||
|
GX40NiCRSINB35-26 ah a awm. |
1.4852 |
1100 |
|||
|
GX50NICRCO20-20-20 ah a awm. |
1.4874 |
1150 |
|||
|
GX50NICRCOW35-25-15-5 ah hian a awm a. |
1.4869 |
1200 |
|||
|
GX40NICRRNB45-35 ah hian a awm a. |
1.4889 |
1160 |
|||
|
Nickel leh . |
Cobalt base a ni a . |
Alloys 1000 a ni. |
G-nirr28w a ni. |
2.4879 |
1150 |
|
G-cocr28 a ni. |
2.4778 |
1200 a |
|||
|
g-nirr50nb a ni. |
2.4680 |
1050 b |
|||
|
G-NICR-15 a ni. |
2.4815 |
1100 |
|||
|
A Cyclic Heatings tan chuan boruak a lum ber chu 1100 c a ni. B He grade hi oil-ash attack a nih chuan a lum ber 950℃thlenga hman a ni . |
|||||